This International Standard specifies a method of measuring

  • the time required for the temperature of a solution of unsaturated-polyester resin and a catalyst, heated in a thermostatically controlled bath at 130 °C, to rise
  • from 80 °C to 140 °C,
  • from 80 °C to the maximum temperature reached;
    • the maximum temperature reached;
    • the speed of the reaction, determined by drawing a tangent at the point of inflection of the temperature/time curve.

It applies in particular to unsaturated-polyester resins processed at a temperature higher than 100 °C.

ORDER

Price:

$52.38        


Want this as a site license?

To find similar documents by classification:

83.080.10 (Thermosetting materials Including ebonite Silicones, see 71.100.55)

This document comes with our free Notification Service, good for the life of the document.

This document is available in either Paper or PDF format.

Document Number

ISO 14848:1998

Revision Level

1ST EDITION

Status

Current

Publication Date

June 1, 1998

Committee Number

ISO TC 61/SC 12/WG 5