AMS-5702 Complete Document History
Nickel Alloy, Corrosion and Heat-Resistant, Bars, Forgings, and Rings, 41.5Ni - 16Cr - 37Fe - 2.9Cb (Nb) - 1.8Ti, Consumable Electrode Remelted or Vacuum Induction Melted, 1750 Deg F (954 Deg C) Solution Heat Treated

Complete Current Edition:
   REVISION F - Nickel Alloy, Corrosion- and Heat-Resistant, Bars, Forgings, Rings and Stock for Forging 41.5Ni - 16Cr - 37Fe - 2.9Cb (Nb) - 1.8Ti Consumable Electrode Remelted or Vacuum Induction Melted 1750 °F (954 °C) Solution Heat Treated - Dec. 13, 2023

Obsolete Revision Information:
   REVISION E - Nickel Alloy, Corrosion and Heat-Resistant, Bars, Forgings, and Rings, 41.5Ni - 16Cr - 37Fe - 2.9Cb (Nb) - 1.8Ti, Consumable Electrode Remelted or Vacuum Induction Melted, 1750 °F (954 °C) Solution Heat Treated - Feb. 12, 2018
   REVISION D R12 - REAFFIRMED IN 2012 - April 1, 2012
   REVISION D - Nickel Alloy, Corrosion and Heat-Resistant, Bars, Forgings, - Jan. 1, 2007
   REVISION C - Nickel Alloy, Corrosion and Heat-Resistant, Bars, Forgings, - April 1, 1993
   REVISION B - OBSOLETE REVISION BY REQUEST - Jan. 1, 1988
   REVISION A - OBSOLETE REVISION BY REQUEST - July 1, 1987
   BASE - OBSOLETE REVISION BY REQUEST - Nov. 1, 1971