ASTM-D3762 Standard Test Method for Adhesive-Bonded Surface Durability of Aluminum (Wedge Test) (Withdrawn 2019)

ASTM-D3762 - 2003 R10 EDITION - CANCELLED
Show Complete Document History

Document Center Inc. is an authorized dealer of ASTM standards.
The following bibliographic material is provided to assist you with your purchasing decision:

Standard Test Method for Adhesive-Bonded Surface Durability of Aluminum (Wedge Test) (Withdrawn 2019)

Scope

1.1 This test method , simulates in a qualitative manner the forces and effects on an adhesive bond joint at metal-adhesive/primer interface. It has proven to be highly reliable in determining and predicting the environmental durability of adherend surface preparations. The method has proven to be correlatable with service performance in a manner that is much more reliable than conventional lap shear or peel tests (Note 2).

Note 1—While this test method is intended for use in aluminum-to-aluminum applications it may be used for determining surface durability of other metals and plastics provided consideration is given to thickness and rigidity of the adherends.

Note 2—This test method is not a quantitative fracture strength test method. To measure fracture strength see Test Method D3433.

1.2 The values stated in SI units are to be regarded as the standard. The values given in parentheses are for information only.

1.3 This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety and health practices and determine the applicability of regulatory limitations prior to use.

Significance and Use

The test is primarily qualitative, but is very discriminating in determining variations in adherend surface preparation parameters and adhesive environmental durability. The test has found application in controlling surface preparation operations and in screening surface preparations, primer and adhesive systems for durability. In addition to determining crack growth rate and assigning a value to it, the adhesivejoint failure is evaluated and reported. For example, adhesion failure; cohesion failure; or adherend failure are noted after opening up the specimen at the conclusion of the test period.

Keywords

adhesive; crack extension; durability; surface preparation; wedge; Wedge test; Adhesive bonds; Adhesive joints; Adhesive joints--metal-to-metal; Aluminum; Durability--adhesives; Fracture testing--adhesive bonds; Metallic adhesives; Metal-to-metal contact; Surface analysis--adhesives/tape

To find similar documents by ASTM Volume:

15.06 (Adhesives)

To find similar documents by classification:

83.180 (Adhesives Including adhesive tapes Adhesive tapes for electrical insulation purposes, see 29.035.20)

This document comes with our free Notification Service, good for the life of the document.

This document is available in either Paper or PDF format.

 

Customers who bought this document also bought:

QPL-81706
Chemical Conversion Materials for Coating Aluminum and Aluminum Alloys

QPL-AMS-2644
Inspection Material, Penetrant

ASTM-E18
Standard Test Methods for Rockwell Hardness of Metallic Materials

Document Number

ASTM-D3762-03(2010)

Revision Level

2003 R10 EDITION

Status

Cancelled

Modification Type

Withdrawn

Publication Date

Sept. 1, 2010

Document Type

Test Method

Page Count

5 pages

Committee Number

D14.80