ASTM-E2009 › Standard Test Methods for Oxidation Onset Temperature of Hydrocarbons by Differential Scanning Calorimetry
The following bibliographic material is provided to assist you with your purchasing decision:
Scope
1.1 These test methods describe the determination of the oxidative properties of hydrocarbons by differential scanning calorimetry or pressure differential scanning calorimetry under linear heating rate conditions and are applicable to hydrocarbons, which oxidize exothermically in their analyzed form.
1.2 Test Method A—A differential scanning calorimeter (DSC) is used at ambient pressure of one atmosphere of oxygen.
1.3 Test Method B—A pressure DSC (PDSC) is used at high pressure (e.g., 3.5 MPa (500 psig) of oxygen).
1.4 Test Method C—A differential scanning calorimeter (DSC) is used at ambient pressure of one atmosphere of air.
1.5 Units—The values stated in SI units are to be regarded as standard. No other units of measurement are included in this standard.
1.6 This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety, health, and environmental practices and determine the applicability of regulatory limitations prior to use.
1.7 This international standard was developed in accordance with internationally recognized principles on standardization established in the Decision on Principles for the Development of International Standards, Guides and Recommendations issued by the World Trade Organization Technical Barriers to Trade (TBT) Committee.
Significance and Use
5.1 Oxidation onset temperature is a relative measure of the degree of oxidative stability of the material evaluated at a given heating rate and oxidative environment (e.g., oxygen); the higher the OOT value the more stable the material. The OOT is described in Fig. 1. The OOT values can be used for comparative purposes and are not an absolute measurement, like the oxidation induction time (OIT) at a constant temperature (see Test Method E1858). The presence or effectiveness of antioxidants may be determined by these test methods.
FIG. 1 DSC Oxidation (Extrapolated) Onset Temperature (OOT)
5.2 Typical uses of these test methods include the oxidative stability of edible oils and fats (oxidative rancidity), lubricants, greases, and polyolefins.
Keywords
differential scanning calorimetry; differential thermal analysis; hydrocarbons; oxidation; oxidation induction time (OIT); oxidation onset temperature (OOT); oxidative stability; pressure differential scanning calorimetry;
To find similar documents by ASTM Volume:
14.01 (Healthcare Informatics)
To find similar documents by classification:
This document comes with our free Notification Service, good for the life of the document.
This document is available in either Paper or PDF format.
Customers who bought this document also bought:
JAPANESE PHARMACOPOEJapanese Pharmacopoeia - English Edition
IEC-60601-1
Medical electrical equipment - Part 1: General requirements for basic safety and essential performance
IEC-60529
Degrees of protection provided by enclosures (IP Code)
Document Number
ASTM-E2009-23
Revision Level
2023 EDITION
Status
Current
Modification Type
Revision
Publication Date
Feb. 2, 2023
Document Type
Test Method
Page Count
6 pages
Committee Number
E37.01