ISO-806 Aluminium oxide primarily used for the production of aluminium - Determination of loss of mass at 300 degrees C and 1 000 degrees C

ISO-806 - 2ND EDITION - CURRENT
Show Complete Document History

Document Center Inc. is an authorized dealer of ISO standards.
The following bibliographic material is provided to assist you with your purchasing decision:


ISO 806:2004 specifies a method for the determination of loss of mass on heating of aluminium oxide at 300 °C and further loss of mass on ignition at 1 000 °C. By industry convention, these mass losses are often referred to as "moisture (MOI)" and "loss on ignition (LOI)" respectively.

This method is suitable for calcined alumina in the range 0,2 % to 5 % loss of mass at 300 °C and 0,1 % to 2 % loss of mass at 1 000 °C.

This method provides for samples to be treated on an "as-received" basis for determination of actual MOI and LOI in alumina samples. To improve precision of analysis in cases where "as-received" results are not required, samples can be "air-equilibrated" prior to analysis. "Air-equilibration" can greatly affect MOI results and significantly alter LOI results. The "air-equilibration" procedure and its effects are discussed.

Instrumental methods are also discussed.

ORDER

Price:

$78.57        


Want this as a site license?

To find similar documents by classification:

71.100.10 (Materials for aluminium production)

This document comes with our free Notification Service, good for the life of the document.

This document is available in either Paper or PDF format.

Document Number

ISO 806:2004

Revision Level

2ND EDITION

Status

Current

Publication Date

Oct. 15, 2004

Committee Number

ISO/TC 226