Nickel Alloy, Corrosion and Heat-Resistant, Bars, Forgings, and Rings 41.5Ni - 16Cr - 37Fe - 2.9Cb (Nb) - 1.8Ti Consumable Electrode Remelted or Vacuum Induction Melted 1800 °F (982 °C) Solution Heat Treated
Complete Current Edition: |
REVISION F - Vacuum Induction Melted 1800 °F (982 °C) Solution Heat Treated - March 9, 2022
|
Obsolete Revision Information: |
REVISION E - Nickel Alloy, Corrosion and Heat-Resistant, Bars, Forgings, and Rings 41.5Ni - 16Cr - 37Fe - 2.9Cb (Nb) - 1.8Ti Consumable Electrode Remelted or Vacuum Induction Melted 1800 °F (982 °C) Solution Heat Treated - July 6, 2015
REVISION D - Nickel Alloy, Corrosion and Heat-Resistant, Bars, Forgings, - Feb. 1, 2007
REVISION C - Nickel Alloy, Corrosion and Heat-Resistant, Bars, Forgings, - April 1, 1993
REVISION B - OBSOLETE REVISION BY REQUEST - Jan. 1, 1988
REVISION A - OBSOLETE REVISION BY REQUEST - April 1, 1981
BASE - OBSOLETE REVISION BY REQUEST - Nov. 1, 1971
|