AMS-5703 Complete Document History
Nickel Alloy, Corrosion and Heat-Resistant, Bars, Forgings, and Rings, 41.5Ni - 16Cr - 37Fe - 2.9Cb - 1.8Ti, Consumable Electrode or Vacuum Induction Melted, 1750 Deg F (954 Deg C) Solution, Stabilization, and Precipitation Heat Treated

Complete Current Edition:
   REVISION E - Consumable Electrode or Vacuum Induction Melted 1750 °F (954 °C) Solution, Stabilization, and Precipitation Heat Treated - March 4, 2018

Obsolete Revision Information:
   REVISION D R12 - REAFFIRMED IN 2012 - Feb. 1, 2012
   REVISION D - Nickel Alloy, Corrosion and Heat-Resistant, Bars, Forgings, - Sept. 1, 2006
   DOD ADOPTION - FYI ONLY: DOD ADOPTED - March 28, 2006
   REVISION C - Nickel Alloy, Corrosion and Heat-Resistant, Bars, Forgings, - July 1, 1993
   REVISION B - OBSOLETE REVISION BY REQUEST - Jan. 1, 1988
   REVISION A - OBSOLETE REVISION BY REQUEST - July 1, 1981
   BASE - OBSOLETE REVISION BY REQUEST - Nov. 1, 1971