AMS-5731 Complete Document History
Steel, Corrosion and Heat-Resistant, Bars, Wire, Forgings, Tubing, and Rings, 15Cr - 25.5Ni - 1.2Mo - 2.1Ti - 0.006B - 0.30V, Consumable Electrode Melted, 1800 Deg F (982 Deg C) Solution Heat Treated

Complete Current Edition:
   REVISION M - Treated Precipitation Hardenable - Sept. 5, 2023

Obsolete Revision Information:
   REVISION L R18 - REAFFIRMED IN 2018 - Oct. 10, 2018
   REVISION L R12 - REAFFIRMED IN 2012 - July 1, 2012
   REVISION L - Steel, Corrosion and Heat-Resistant, Bars, Wire, Forgings, T - June 1, 2006
   REVISION K - Steel, Corrosion and Heat-Resistant, Bars, Wire, Forgings, T - Oct. 1, 2001
   REVISION J - Steel, Corrosion and Heat-Resistant, Bars, Wire, Forgings, T - May 1, 1995
   DOD ADOPTION - FYI ONLY: DOD ADOPTED - Aug. 15, 1990
   REVISION H - Steel, Corrosion and Heat-Resistant, Bars, Wire, Forgings, T - July 1, 1989
   REVISION G - OBSOLETE REVISION BY REQUEST - April 1, 1984
   REVISION F - OBSOLETE REVISION BY REQUEST - July 1, 1983
   REVISION E - OBSOLETE REVISION BY REQUEST - Jan. 1, 1976
   REVISION D - OBSOLETE REVISION BY REQUEST - Nov. 1, 1969
   REVISION C - OBSOLETE REVISION BY REQUEST - April 1, 1967
   REVISION B - OBSOLETE REVISION BY REQUEST - March 1, 1966
   REVISION A - OBSOLETE REVISION BY REQUEST - Jan. 1, 1964
   BASE - OBSOLETE REVISION BY REQUEST - Jan. 1, 1963