ASTM-B183 Standard Practice for Preparation of Low-Carbon Steel for Electroplating

ASTM-B183 - 2018 EDITION - CURRENT
Show Complete Document History

Document Center Inc. is an authorized dealer of ASTM standards.
The following bibliographic material is provided to assist you with your purchasing decision:


This practice provides an aid for setting up a suitable cleaning cycle preparatory to electroplating of low-carbon steel and indicates some of the precautions that must be taken to maintain this cycle in good operating condition. The preparatory procedure involves three basic steps in the following order: (1) removal of oils, grease, and caked-on dirt; (2) removal of scale and oxide films by pickling; and (3) removal of any smut left on the surface and activation of the steel. The cleaning of racked parts, which shall subsequently be electroplated in still tanks, agitated tanks, and semi- and full-automatic equipment, should be performed following this cycle: (1) precleaning; (2) electrocleaning; (3) water rinse; (4) acid pickling; (5) alkaline descaling; and (6) water rinse. Parts in bulk, which shall subsequently be electroplated in hand-operated or automatic barrels, should follow this cleaning cycle: (1) alkaline cleaning; (2) water rinse; (3) acid pickling; and (4) water rinse.

ORDER

Price:

$44.00        

Changes from the previous issue

A redline edition is available for this document, with all changes visible. Ask Document Center Inc. for more information.

Scope

1.1 This practice is intended as an aid to electroplaters in setting up a suitable cleaning cycle preparatory to electroplating of low-carbon steel (Note 1) containing less than 0.35 mass % of carbon and to indicate some of the precautions that must be taken to maintain this cycle in good operating condition.

Note 1: The preparation of high-carbon steel for electroplating is covered in Guide B242.

1.2 The values stated in SI units are to be regarded as standard. No other units of measurement are included in this standard.

1.3 This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety, health, and environmental practices and determine the applicability of regulatory limitations prior to use.

1.4 This international standard was developed in accordance with internationally recognized principles on standardization established in the Decision on Principles for the Development of International Standards, Guides and Recommendations issued by the World Trade Organization Technical Barriers to Trade (TBT) Committee.

Keywords

ICS Number Code 25.220.10 (Surface preparation)

To find similar documents by ASTM Volume:

02.05 (Metallic and Inorganic Coatings; Metal Powders and Metal Powder Products)

To find similar documents by classification:

25.220.10 (Surface preparation Including surface preparation for painting, cleaning, scouring, blasting, etc.)

This document comes with our free Notification Service, good for the life of the document.

This document is available in either Paper or PDF format.

Document Number

ASTM-B183-18

Revision Level

2018 EDITION

Status

Current

Modification Type

Revision

Publication Date

June 1, 2018

Document Type

Practice

Page Count

3 pages

Committee Number

B08.02