ASTM-B367 Historical Revision Information
Standard Specification for Titanium and Titanium Alloy Castings

ASTM-B367 - 2013 R17 EDITION - SUPERSEDED
Show Complete Document History

Document Center Inc. is an authorized dealer of ASTM standards.
The following bibliographic material is provided to assist you with your purchasing decision:


This specification covers the standard requirements for titanium and titanium alloy castings intended for general corrosion resistant and industrial applications. Materials for this specification shall be melted by conventional processes used for reactive metals such as consumable electrode and induction-slag, plasma arc, induction-skull, and electron beam melting processes. The materials shall undergo chemical, pour, and product analysis to determine the chemical composition which shall conform to the requirements for nitrogen, carbon, hydrogen, iron, oxygen, aluminum, vanadium, tin, ruthenium, palladium, cobalt, molybdenum, chromium, nickel, niobium, zirconium, silicon, and titanium. All castings shall be supplied in the as-cast condition except when post-weld heat treatment is required wherein it shall consist of a stress relief performed at certain temperatures. The surface of the castings shall be free of adhering mold material, scale, cracks, and hot tears as determined by visual inspection.

ORDER

Scope

1.1 This specification covers titanium and titanium alloy castings intended for general corrosion resistant and industrial applications. as follows:

1.1.1 Grade C-2—UNS R52550. Unalloyed titanium,

1.1.2 Grade C-3—UNS R52550. Unalloyed titanium,

1.1.3 Grade C-5—UNS R56400. Titanium alloy (6 % aluminum, 4 % vanadium),

1.1.4 Grade C-7—UNS R52700. Unalloyed titanium plus 0.12 to 0.25 % palladium,

1.1.5 Grade C-8—UNS R52700. Unalloyed titanium plus 0.12 to 0.25 % palladium,

1.1.6 Grade C-9—UNS R56320. Titanium alloy (3 % aluminum, 2.5 % vanadium),

1.1.7 Grade C-12—UNS R53400. Titanium alloy (0.3 % molybdenum, 0.8 % nickel),

1.1.8 Grade C-16—UNS R52402. Unalloyed titanium plus 0.04 to 0.08 % palladium,

1.1.9 Grade C-17—UNS R52252. Unalloyed titanium plus 0.04 to 0.08 % palladium, and

1.1.10 Grade C-38—UNS R54250. Titanium alloy (4 % aluminum, 2.5 % vanadium, 1.5 % iron).

1.2 This specification is intended for use of purchasers and/or producers of reactive metal castings for defining the requirements and assuring the properties of castings for unique corrosion-resistant applications, that is, not for commodity items which must meet all potential purchasers’ requirements.

1.2.1 Users are advised to use the specification as a basis for obtaining castings which will meet minimum acceptance requirements established and revised by consensus of the members of the committee.

1.2.2 User requirements considered more stringent may be met by the addition to the purchase order of one or more supplementary requirements, which may include, but are not limited to, those listed in Sections S1 through S8.

1.3 The values stated in inch-pound units are to be regarded as standard. The values given in parentheses are mathematical conversions to SI units that are provided for information only and are not considered standard.

1.4 This international standard was developed in accordance with internationally recognized principles on standardization established in the Decision on Principles for the Development of International Standards, Guides and Recommendations issued by the World Trade Organization Technical Barriers to Trade (TBT) Committee.

Keywords

castings; corrosion resistant; titanium; titanium alloys;

To find similar documents by ASTM Volume:

02.04 (Nonferrous Metals--Nickel, Cobalt, Lead, Tin, Zinc, Cadmium, Precious, Reactive, Refractory Metals and Alloys; Materials for Thermostats, Electrical Heating and Resistance Contacts, and Connectors)

To find similar documents by classification:

77.150.50 (Titanium products)

This document comes with our free Notification Service, good for the life of the document.

This document is available in either Paper or PDF format.

Document Number

ASTM-B367-13(2017)

Revision Level

2013 R17 EDITION

Status

Superseded

Modification Type

Reapproval

Publication Date

Nov. 1, 2017

Document Type

Specification

Page Count

6 pages

Committee Number

B10.01