Standard Test Method for Adhesive-Bonded Surface Durability of Aluminum (Wedge Test)

ASTM-D3762 - 2003 EDITION - SUPERSEDED
Show Complete Document History

Document Center Inc. is an authorized dealer of ASTM standards.
The following bibliographic material is provided to assist you with your purchasing decision:

Standard Test Method for Adhesive-Bonded Surface Durability of Aluminum (Wedge Test) (Withdrawn 2019)
ORDER

Scope

1.1 This test method, simulates in a qualitative manner the forces and effects on an adhesive bond joint at metal-adhesive/primer interface. It has proven to be highly reliable in determining and predicting the environmental durability of adherend surface preparations. The method has proven to be correlatable with service performance in a manner that is much more reliable than conventional lap shear or peel tests (Note 2).

Note 1W—hile this test method is intended for use in aluminum-to-aluminum applications it may be used for determining surface durability of other metals and plastics provided consideration is given to thickness and rigidity of the adherends.

Note 2—This test method is not a quantitative fracture strength test method. To measure fracture strength see Test Method D 3433.

1.2 The values stated in SI units are to be regarded as the standard. The values given in parentheses are for information only.

1.3 This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety and health practices and determine the applicability of regulatory limitations prior to use.

Significance and Use

The test is primarily qualitative, but is very discriminating in determining variations in adherend surface preparation parameters and adhesive environmental durability. The test has found application in controlling surface preparation operations and in screening surface preparations, primer and adhesive systems for durability. In addition to determining crack growth rate and assigning a value to it, the adhesivejoint failure is evaluated and reported. For example, adhesion failure; cohesion failure; or adherend failure are noted after opening up the specimen at the conclusion of the test period.

Keywords

adhesive; crack extension; durability; surface preparation; wedge; ICS Number Code 83.180 (Adhesives)

To find similar documents by ASTM Volume:

15.06 (Adhesives)

To find similar documents by classification:

83.180 (Adhesives Including adhesive tapes Adhesive tapes for electrical insulation purposes, see 29.035.20)

This document comes with our free Notification Service, good for the life of the document.

This document is available in either Paper or PDF format.

Document Number

ASTM-D3762-03

Revision Level

2003 EDITION

Status

Superseded

Modification Type

Revision

Publication Date

Aug. 10, 2003

Document Type

Test Method

Page Count

5 pages

Committee Number

D14.80