ASTM-D6931 › Historical Revision Information
Standard Test Method for Indirect Tensile (IDT) Strength of Bituminous Mixtures
The following bibliographic material is provided to assist you with your purchasing decision:
Scope
1.1 This test method covers procedures for preparing and testing laboratory-fabricated or field-recovered cores of bituminous mixtures to determine the Indirect Tensile (IDT) Strength.
1.2 The within-laboratory repeatability standard deviation, for the recommended rate of loading (50 mm/min) and test temperature (25ºC), has been determined to be 80 kPa for 101.6 mm diameter specimens, based on 28 labs using either 2 or 4 test replicates with 11 different mix samples. Additional data is provided in Table 1 for the user’s information. The between-laboratory reproducibility of this test method is being determined and will be available on or before August 2012. Therefore, this test method should not be used for acceptance or rejection of materials for purchasing purposes.
1.3 The values stated in SI units are to be regarded as standard.
1.4 This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety and health practices and determine the applicability of regulatory limitations prior to use.
Source of Data | Number of Replicates | Specimen Diameter (mm) | Loading Rate (mm/min) | Test Temperature (°C) | Average Strength (kPa) | Standard Deviation Strength (kPa) | d2s (2.83×SE) (kPa) | Standard Deviation Strength (% mean) | d2s (2.83×SE) (% mean) |
---|---|---|---|---|---|---|---|---|---|
Anderson and McGennisA | 3 | 150 | 12.5 | -10 | 2870 | 200 | 566 | 7.0 | 19.8 |
N CHRP Report 530B | 3 | 150 | 12.5 | -10 | - | - | - | 9 | 22–32 |
(4 aggregate types; 4 binders) | 2 | 150 | 12.5 | -10 | - | - | - | 11 | |
(nom max size: 9.5 mm to 25 mm) | |||||||||
Solaimanian and KennedyC | 4 | 100 | 50 | 25 | - | 103 | 292 | – | – |
moisture-conditioned | 50 | 25 | - | 83 | 234 | – | – | ||
(9 labs; 3 aggregate types; 2 binders) | |||||||||
Test Method D4867/D4867M (dry or conditioned) | 2 | 100 | 50 | 25 | - | 55 | 159 | – | – |
(19 labs; 5 mixtures) | |||||||||
Suggested Single Lab Precision | 50 | 25 | 80 |
A R. M. Anderson and R. B. McGennis, “Ruggedness Evaluation of AASHTO TP7 and TP9,” Phase I, FHWA HIPT (Task J), Federal Highway Administration, November 1998.
B W. Christensen and R. F. Bonaquist, “Evaluation of Indirect Tensile Test (IDT) Procedures for Low-Temperature Performance of Hot Mix Asphalt,” NCHRP Report 530.
C Solaimanian and T. W. Kennedy, “Precision of the Moisture Susceptibility Test Method TEX-531-C,” Project Summary Report 4909-S, November 2000.
Significance and Use
The values of IDT strength may be used to evaluate the relative quality of bituminous mixtures in conjunction with laboratory mix design testing and for estimating the potential for rutting or cracking. The results can also be used to determine the potential for field pavement moisture damage when results are obtained on both moisture-conditioned and unconditioned specimens.
Keywords
asphalt mixture; bituminous mixture; indirect tensile strength; IDT; Bituminous materials/applications; IDT (indirect tensile strength); Indirect tensile strength (IDT); Tensile strength; ICS Number Code 93.080.20 (Road construction materials)
To find similar documents by ASTM Volume:
04.03 (Road and Paving Materials; Vehicle-Pavement Systems)
To find similar documents by classification:
93.080.20 (Road construction materials Including asphalts, road pavements, etc.)
This document comes with our free Notification Service, good for the life of the document.
This document is available in either Paper or PDF format.
Document Number
ASTM-D6931-12
Revision Level
2012 EDITION
Status
Superseded
Modification Type
Revision
Publication Date
March 31, 2012
Document Type
Test Method
Page Count
5 pages
Committee Number
D04.26