Scope

1.1  This practice incorporates etching and metallographic examination of Wrought Nickel-Rich, Chromium, Molybdenum-Bearing Alloys such as, but not limited to, UNS N06686 and UNS N10276.

1.2  Microstructures have a strong influence on properties and successful application of metals and alloys. The presence of mu-phase in the microstructure may significantly reduce the corrosion resistance of Wrought Nickel-Rich, Chromium, and Molybdenum-Bearing Alloys.

1.3 This practice may be used to determine the presence of mu-phase in Wrought Nickel-Rich, Chromium, and Molybdenum-Bearing Alloys through comparison of microstructure observed for etched metallographic specimens to a glossary of photomicrographs displaying the presence and absence of mu-phase in the microstructure.

1.4 The values stated in SI units are to be regarded as the standard. Other units are given in parentheses for information only.

1.5 This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety and health practices and determine the applicability of regulatory limitations prior to use.

Significance and Use

4.1 These test methods describe laboratory tests to determine the presence of mu-phase in Wrought Nickel-Rich, Chromium, and Molybdenum-Bearing Alloys through comparison of microstructure observed for etched metallographic specimens to a glossary of photomicrographs displaying the presence and absence of mu-phase in the microstructure. The presence of mu-phase in the microstructure may significantly reduce the corrosion resistance, strength, toughness and ductility of Wrought Nickel-Rich, Chromium, and Molybdenum-Bearing Alloys.

Keywords

corrosion; ferric chloride test solution; localized corrosion; microstructure; mu-phase; nickel–base alloys; pitting; properties; stainless steels; ICS Number Code 77.040.30 (Chemical analysis of metals)

To find similar documents by ASTM Volume:

03.02 (Corrosion of Metals; Wear and Erosion)

To find similar documents by classification:

77.040.30 (Chemical analysis of metals Chemical analysis in general, see 71.040.40 Chemical analysis of ferrous metals, see 77.080 Chemical analysis of ferroalloys, see 77.100 Chemical analysis of non-ferrous metals, see 77.120 Chemical analysis of sintered metals and hard metals, see 77.160)

This document comes with our free Notification Service, good for the life of the document.

This document is available in either Paper or PDF format.

Document Number

ASTM-G209-12a

Revision Level

2012A EDITION

Status

Superseded

Modification Type

Revision

Publication Date

Dec. 15, 2012

Document Type

Practice

Page Count

9 pages

Committee Number

G01.05