IEC 62804-1-1:2020 defines procedures to test and evaluate for potential-induced degradation-delamination (PID-d) mode in the laminate of crystalline silicon PV modules-principally those with one or two glass faces. This document evaluates delamination attributable to current transfer between ground and the module cell circuit. Elements driving the delamination that this test is designed to actuate include reduced adhesion associated with damp heat exposure, sodium accumulation at interfaces, and cathodic gas evolution in the cell circuit, metallization, and other components within the PV module activated by the voltage potential. The change in power of crystalline silicon PV modules associated with the stress factors applied (the purview of IEC TS 62804-1) is not considered in the scope.
To find similar documents by classification:
27.160 (Solar energy engineering Including photovoltaic energy systems)
This document comes with our free Notification Service, good for the life of the document.
This document is available in either Paper or PDF format.
Document Number
IEC/TS 62804-1-1 Ed. 1.0 en:2020
Revision Level
EDITION 1.0
Status
Current
Publication Date
Jan. 1, 2020
Committee Number
82