AMS-5702 › Historical Revision Information
Nickel Alloy, Corrosion- and Heat-Resistant, Bars, Forgings, Rings and Stock for Forging 41.5Ni - 16Cr - 37Fe - 2.9Cb (Nb) - 1.8Ti Consumable Electrode Remelted or Vacuum Induction Melted 1750 °F (954 °C) Solution Heat Treated
Nickel Alloy, Corrosion and Heat-Resistant, Bars, Forgings, and Rings, 41.5Ni - 16Cr - 37Fe - 2.9Cb (Nb) - 1.8Ti, Consumable Electrode Remelted or Vacuum Induction Melted, 1750 Deg F (954 Deg C) Solution Heat Treated
This document comes with our free Notification Service, good for the life of the document.
This document is available in either Paper or PDF format.
Document Number
AMS5702F
Revision Level
REVISION F
Status
Current
Publication Date
Dec. 13, 2023