Standard Test Method for Apparent Hoop Tensile Strength of Plastic or Reinforced Plastic Pipe by Split Disk Method
The following bibliographic material is provided to assist you with your purchasing decision:
Scope
1.1 This test method covers the determination of the comparative apparent tensile strength of most plastic products utilizing a split disk test fixture, when tested under defined conditions of pretreatment, temperature, humidity, and test machine speed. This test method is applicable to reinforced-thermosetting resin pipe regardless of fabrication method. This test method also is applicable to extruded and molded thermoplastic pipe.
Procedure A is used for reinforced-thermosetting resin pipe; Procedure B is used for thermoplastic pipe of any size; Procedure C is used for thermoplastic pipe with nominal diameter of 4-1/2 in. and greater.
1.2 The values stated in inch-pound units are to be regarded as the standard.
1.3 This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety and health practices and determine the applicability of regulatory limitations prior to use.
Keywords
apparent tensile strength; hoop tensile strength; plastic pipe; split-disk method
To find similar documents by ASTM Volume:
08.04 (Plastic Piping Systems)
To find similar documents by classification:
83.120 (Reinforced plastics Materials for the reinforcement of plastics, see 59.100)
This document comes with our free Notification Service, good for the life of the document.
This document is available in either Paper or PDF format.
Document Number
ASTM-D2290-00e1
Revision Level
2000(E1) EDITION
Status
Superseded
Modification Type
Editorially changed
Publication Date
Nov. 1, 2003
Document Type
Test Method
Page Count
5 pages
Committee Number
F17.40